Stainless Steel - Grade 316 (UNS S31600)

Feb 02, 2026

Legg igjen en beskjed

1.4833 Stainless Steel Plate & Coil: Austenitic Heat-Resistant High-Strength Plate/Coil1.4541 Stainless Steel Plate & Coil: Austenitic Titanium-Stabilized High-Temp Welding Plate/Coil1.4306 Stainless Steel Plate & Coil: Austenitic Ultra-Low Carbon Welding-Friendly Plate/Coil

Grade 316L, the low carbon version of 316 and is immune from sensitisation (grain boundary carbide precipitation). Thus it is extensively used in heavy gauge welded components (over about 6mm). Grade 316H, with its higher carbon content has application at elevated temperatures, as does stabilised grade 316Ti.

The austenitic structure also gives these grades excellent toughness, even down to cryogenic temperatures.

These properties are specified for flat rolled product (plate, sheet and coil) in ASTM A240/A240M. Similar but not necessarily identical properties are specified for other products such as pipe and bar in their respective specifications.

Table 1. Composition ranges for 316 grade of stainless steels.

  C P S N
316 - - - 0 - 16.0 2.00 10.0 -
0.08 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316L - - - - - 16.0 2.00 10.0 -
0.03 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316H 0.04 0.04 0 - - 16.0 2.00 10.0 -
0.10 0.10 0.75 0.045 0.03 18.0 3.00 14.0 -

 

Table 2. Mechanical properties of 316 grade stainless steels.

Yield Str 0.2% Proof (MPa) min Elong (% in 50 mm) min
316 515 205 40 95 217
316L 485 170 40 95 217
316H 515 205 40 95 217